Heat treatment is where a gear’s durability is decided. The same steel, cut to the same profile, lasts for years with a hardened surface and a tough core, and fails early when the heat treatment is mismatched to the load. Henan Yizhi Machinery Co., Ltd. (YIZHI MACHINERY) applies the three main routes — carburizing and quenching, quenching and tempering, and induction hardening — to the gears and shafts it machine-cuts, chosen from the load, the material, and the accuracy the part has to hold. This guide explains what each route does, how to match one to your gear, and how the result is verified.

Why Gears Need Heat Treatment

A gear tooth spends its life in contact: the flanks carry load every revolution, the surface resists wear, and the core absorbs shock from sudden loads. Plain as-machined steel is too soft to do all of this for long. Heat treatment changes that without changing the shape — it hardens the working surfaces while the core stays tough, which separates a gear that wears evenly for years from one that pits, wears, or breaks early.

The trade-off is control. Steel shifts as it heats and quenches, so distortion is planned into the build rather than added at the end. Heat treatment sits at a fixed point in the production flow, with inspection on either side, and is often followed by grinding to take the distortion back out. Where the step sits relative to the inspection points is laid out on the heat treatment capability page.

The Main Heat Treatment Routes

YIZHI MACHINERY applies three routes, each suited to a different load and material. The choice comes down to the gear’s duty, the steel it is cut from, and the accuracy it has to hold after hardening.

Carburizing and Quenching

For the heaviest tooth contact, the route is carburizing and quenching. A low-carbon alloy steel, around 0.15% to 0.20% carbon with added nickel, chromium, molybdenum, or manganese, is held in a carburizing environment so carbon soaks into the surface, then quenched. The result is a hard case, typically 55 to 60 HRC at the surface with a hardened layer around 1.0 mm deep, over a core that stays tough enough to absorb shock. The greater the load, the deeper the case the drawing calls for.

Quenching and Tempering

Quenching and tempering is the balanced, all-round route. The part is heated, quenched, then tempered to bring the hardness back to a workable mid-range instead of leaving it brittle. It works as pre-treatment before machining and as the finishing route where a part needs uniform strength through the section rather than a hard case over a soft core.

Induction Hardening

Induction hardening heats only the surface with a coil, so hardening stays exactly where the load is while the rest of the part is untouched. It is fast, controlled, and the common route for 45 steel and 42CrMo. The payoff on carbon steel is significant: a 45 steel gear can see its strength rise by roughly four times after the tooth surface is induction hardened, with the accuracy, such as the tooth pitch error, dropping by about one grade. The control point is preventing cracks and warping, which is why the heating is kept tight.

Matching the Route to the Gear

The choice comes down to three things: the load on the tooth, the material, and the accuracy the finished part has to hold. A gear that carries heavy contact load on its flanks — worm gears, heavily loaded helical and herringbone gears, planetary ring gears and planet pinions — goes down the carburizing route, so the surface that meets the load is the hard part.

Straight bevel gear with machined tooth profile

A shaft or gear in 45 steel or 42CrMo that needs a hard surface over a tougher body is a candidate for induction hardening; the custom gear shaft is the typical example. Where the load is moderate and spread, or a uniform mid-range hardness is needed, quenching and tempering is the route. Material and route are specified together on the drawing: carbon steel for mechanical structures is the most common starting point and takes induction hardening well; chromium-molybdenum steels are used after quenching, tempering, and induction hardening; low-carbon alloy steels go through carburizing. In worm-gear sets the pairing is a hardened steel worm against a softer bronze wheel.

What Happens After Heat Treatment

Heat treatment is not the last step; it is the step that makes the next ones necessary. Steel shifts as it hardens, so the part that comes out of the furnace is not exactly the part that went in — dimensions move and the tooth profile has to be corrected.

That is why the flow puts inspection on both sides. After the final heat treatment, a metallographic inspection and a hardness test are run together, and the part moves on to grinding only once that passes. Grinding takes the distortion back out and holds the tooth form to the specified accuracy. A part that fails the post-treatment inspection does not move forward; it ends the process.

Precision worm gear set with machined worm and gear wheel

Surface Treatment for Corrosion and Fatigue

Hardness is not the only thing a gear surface has to handle. Corrosion and fatigue are separate failures, treated separately. After the heat treatment, surface treatments are applied as the drawing calls for:

  • Galvanizing and blackening, for corrosion resistance
  • Phosphating, as a base for protection and a finished surface
  • Shot peening, which adds a layer of compressive stress at the surface to improve fatigue life

These are chosen for the environment the part runs in. Galvanizing or blackening suits a humid or chemical environment; shot peening suits cyclic loading, putting a compressive surface layer in to improve fatigue life. Surface treatment is specified alongside the heat treatment, not decided at the end.

How Heat-Treated Gears Are Inspected

The value of the heat treatment is only as good as the checking around it. Inspection covers the things that matter for a hardened part: surface hardness against the specification, the depth of the hardened case, the metallographic structure, and, once ground, the tooth profile, pitch, and runout against ISO 1328.

Most work is made to ISO 1328 grades 6 to 8, with some parts at grade 5, and the inspection plan matches the grade. A gear measuring machine checks profile and pitch, a coordinate measuring machine checks dimensions, and a hardness tester confirms the case. Because hardening can shift a part out of tolerance, the grind that follows brings the accuracy back to the stated grade. The logic at every inspection point is the same: a failure ends the process, a pass moves the part on.

Conclusion

Heat treatment is where a gear’s service life is decided: a hard case over a tough core, matched to the load and the material, held to the accuracy the part has to run at. Carburizing and quenching builds the deep case for the heaviest tooth contact; quenching and tempering gives balanced mid-range hardness; induction hardening puts a controlled hard surface on 45 steel and 42CrMo parts. Whatever the route, the part is inspected before and after, and ground where the tooth form has to be true. If you are specifying gears or shafts and want the heat treatment matched to the load and verified to ISO 1328, reach out to our team to start a custom build from your drawings.

Frequently Asked Questions

Q: What does heat treatment do to a gear?

It changes the surface and the core without changing the shape: the working surfaces harden to resist wear, the core stays tough to absorb shock. The trade-off is that the part shifts as it hardens, so it is usually ground afterward to bring the accuracy back.

Q: How hard does carburizing make the surface, and how deep?

Typically 55 to 60 HRC at the surface, with a hardened case around 1.0 mm deep. The greater the load, the deeper the layer the drawing calls for. It is used on low-carbon alloy steels that have to run hard on the tooth flanks while keeping a tough core.

Q: What is the difference between induction hardening and carburizing?

Induction hardening heats only the surface with a coil, so hardening stays exactly where the load is; it is the common route for 45 steel and 42CrMo. Carburizing soaks carbon into a low-carbon alloy steel before quenching, building a deeper, harder case for the heaviest tooth contact. The choice comes down to the material and the load.

Q: Can heat treatment change a gear’s accuracy?

Yes. Steel distorts as it is quenched and tempered, so dimensions and the tooth profile shift. The part is inspected after treatment and ground to take the distortion out and hold the profile to the specified accuracy. On 45 steel, induction hardening can raise the strength by about four times while the tooth pitch error drops by about one grade, which the following grind corrects.

Free Quote